What is API 5L X65 Pipe

What is API 5L X65 Pipe

X65 belongs to the high-strength pipeline steel grade in the API 5L standard. Its minimum yield strength reaches 448MPa, which can withstand high-pressure transportation environments and is particularly suitable for the construction of long-distance oil and gas pipelines.

 

What is Carbon Steel API 5L X65 Pipe Specification

Carbon Steel API 5L X65 Pipe Specification

 

What is the Chemical Composition of API 5L X65 PSL 1 Carbon Steel Line Pipes

C P S V
max.b min. max. max. max. max. max.
0.28e 1.40e 0.030 0.030 f f f
0.26 1.45e 0.030 0.030 f f f

 

What is the Chemical Composition  of API 5L X65 PSL 2 Carbon Steel Line Pipes

P S V
L450Q or X65Q 0.18f 0.45f 1.7f 0.025 0.015 g g g h 0.43 0.25
L450M OR X65M 0.12f 0.45f 1.6f 0.025 0.015 g g g h 0.43 0.25

 

What is the Mechanical Properties of API 5L X65 PSL 1 Carbon Steel Line Pipes

Y.S T.S
450(65 300) 535(77 600) F

 

What is the Mechanical Properties of API 5L X65 PSL 2 Carbon Steel Line Pipes

Y.S T.S
450(65 300) 600(87 000) 23%